Home / Automotive / Thermal management and e-drive
Growth programme
Keep the pack in its window.
An electric vehicle manages heat in more places than an engine ever did: battery, motor, inverter, charger and cabin all sit on one coolant network with valves, pumps, manifolds and chillers. Every wetted part sees hot glycol under pressure for the life of the vehicle, and that is exactly the environment in which hydrolysis-resistant CiLON® PA66 and NovaLYN™ mPPE have already proved themselves in radiator end tanks and cooling pipes.
What the material must deliver.
Glycol at temperature, for years
Property retention after coolant ageing is the pass mark; hydrolysis-resistant PA66 and mPPE are specified for it.
Burst and thermal cycling
Manifolds and connectors survive pressure cycling and –40 to +120 °C cycling without leak or creep.
Density and integration
mPPE is the lightest option; both families integrate ports, brackets and sensors into one moulding.
Welded and sealed
Vibration- and laser-weldable grades for two-shell manifolds; sealing surfaces held flat by low-warpage formulations.
Our recommendation, application by application.
| Application | Our recommendation | Grades to start from | Family | Status |
|---|---|---|---|---|
| Coolant manifolds and distribution blocks | mPPE GF30, PA66 GF30 HR HS: no hydrolysis, burst after ageing | 620D3031720C3004 HSHD | NovaLYN™ CiLON® | In development |
| Battery chiller and cooling-plate connectors | PA66 GF30 HR, mPPE GF30: seal geometry held wet | 720C3004 HSHD620D3031 | CiLON® NovaLYN™ | In development |
| Electric water-pump and valve housings | mPPE GF30, PA66 GF30 HR: glycol at 100 °C for life | 620D3031720C3004 HSHD | NovaLYN™ CiLON® | In development |
| Thermostat and multi-way valve housings | PA66 GF30 HR HS: coolant ageing, creep at seals | 720C3004 HSHD720C3004 HS | CiLON® | Ready to specify |
| Radiator and chiller end tanks | PA66 GF30 HR, mPPE GF30: proven crimp and burst life | 720C3004 HSHD620D3031 | CiLON® NovaLYN™ | In production |
| E-motor bearing cages and resolver holders | PA66 GF25–30 HS, PBT GF30: heat ageing, precision | 720C3004 HS730C3001 | CiLON® ZiLITE® | In development |
| Inverter and e-axle sensor housings | PBT GF30, PBT GF30 FR: dimensional stability, V-0 | 730C3001730C3001F | ZiLITE® | In development |
| Cooling-fan modules for battery packs | PA6 GF30 HF, mPPE GF30: flow for thin ribs, low inertia | 710C2031 HFHS620D3031 | CiLON® NovaLYN™ | Ready to specify |
In production: grades in series supply for the named part. Ready to specify: validated grades with data sheets and trial quantities available; part-specific validation is run with you. In development: grades, colours and references being built with OEM and Tier-1 partners.
Design and development notes.
Validate on coolant, not water
Age test parts in the OEM's coolant at the specified concentration and temperature; glycol ageing is more severe than water for polyamide.
Weld-line strength governs burst
For welded manifolds, place gates so weld lines avoid ports and mounting bosses and validate burst pressure on welded assemblies.
Choose mPPE where the geometry moves
Where crimp seals or quick-connect geometry must not change with humidity, NovaLYN™ mPPE holds dimensions that polyamide cannot.
The rest of the growth programme.
Supplied under IATF 16949.
PPAP documentation, IMDS material data and a test certificate with every lot.