Calco Poly Technik

Home / Solutions / Survive heat, coolant and oil

Fifteen years in hot glycol. Choose the material for it.

Hot glycol is the hardest environment a polyamide meets in the vehicle. We specify hydrolysis-resistant PA66 or modified PPE for it, and report retention after ageing in your coolant.

The problem

  • Cracks after coolant ageing

    End-tank cracking at the crimp foot or hose spigot, and loss of crimp force as the material softens with absorbed glycol.

  • Embrittlement over the engine

    Latches, covers and ties that turn brittle after years at under-bonnet temperature.

  • Lost clamp load on the oil side

    Cam covers and oil pans run hot in oil mist for the life of the engine; creep at bolt bosses opens the gasket joint.

The impact

A leak at the crimp or the quick-connector, and a field failure years after the part passed its first tests.

The solution

What we do about it.

Hydrolysis-resistant PA66

CiLON® 720C3004 HSHD is a hydrolysis-resistant, heat-stabilised PA66 with 30% glass fibre, developed to keep tensile strength and part integrity after coolant ageing. It is in series in end tanks and cooling pipes.

Modified PPE where polyamide cannot go

NovaLYN™ 620D3031 does not hydrolyse, absorbs almost no water and holds crimp and bore dimensions wet or dry. It is the lightest option in the circuit.

Heat-stabilised grades

Stabiliser packages selected for retention of tensile strength after ageing at the OEM temperature. Specify them for continuous service above about 120 °C.

Oil-side grades

PA66 with 35% glass fibre, heat stabilised (720C3005HS): oil and heat resistance with the stiffness to keep a gasket flange flat.

Which grade, when.

Choose whenCalco gradeConstructionFamilyWhat it gives you
End tanks, pipes and connectors, standard life target720C3004 HSHDPA66 GF30 HR HSCiLON®Strength after coolant ageing, crimp integrity
Pipes and fittings with lower peak temperature720C3004 HSPA66 GF30 HSCiLON®Heat stabilised, cost-optimised
Aggressive coolant, long life, geometry that must not move620D3031mPPE GF30NovaLYN™No hydrolysis, lowest density, dimensional stability
Cylinder-head covers, oil pans and filter modules720C3005HSPA66 GF35 HSCiLON®Oil and heat resistance, gasket flatness
Covers over the turbo or exhaust side720C3031 HFHSPA66 GF25–30 HF HSCiLON®Higher service temperature with high flow

How we validate it with you.

Coolant ageing

Ageing in the OEM coolant at the specified temperature, typically 1,000 hours at 120–130 °C, with tensile and impact retention reported.

Validate on coolant, not water

Age test parts in the OEM's coolant at the specified concentration and temperature; glycol ageing is more severe than water for polyamide.

Where mPPE is not the answer

Fuels, oils and aromatic solvents attack mPPE; for intake, fuel and oil-side parts, CiLON® polyamide remains the right choice.

Tell us the fluid, the temperature and the life target.

An application engineer replies with a recommended grade, the data behind it and a free 25 kg trial lot.