The problem your part has to solve.
The manifold bolts to a cylinder head running above 100 °C, with peaks well beyond that on turbocharged and hot-side EGR engines. It breathes pulsating vacuum and boost every cycle, and on the inside it carries fuel vapour, blow-by oil mist and, with EGR, acidic condensate. Two- or three-shell designs are vibration- or laser-welded, so the weld seam, the weakest section, sets the burst pressure. Add a throttle-body flange, sensor bosses, resonators and 2–3 mm runner walls, and the material has to fill, weld, seal and survive at once.
Process: Injection moulding, vibration- or laser-welded shells.
What usually goes wrong
- Flange cracking after thermal cycling where weld lines and fibre orientation meet the bolt bosses
- Weld-seam leaks or low burst pressure from poor weld compatibility or glass at the seam
- Warpage that opens the head gasket joint, and embrittlement after heat ageing
- Property loss from condensate hydrolysis on EGR engines
Our recommendation.
For naturally aspirated engines and cost-driven programmes we recommend CiLON® PA6 GF30, 710C3031: the industry's baseline manifold material, with the toughness, weldability and lower melt temperature that make two-shell moulding forgiving. Where continuous temperature passes about 120 °C, or the manifold sits over the turbo or EGR cooler, we move you to PA66 GF35, 720C3001L: PA66's higher melting point and heat-deflection temperature buy the margin. For thin-walled, long runners and laser-welded shells we recommend PA66 GF35 HF HS, 720C3002HFHS: the high-flow package fills 2 mm runner walls without pressure loss, the heat stabiliser protects the aged tensile strength, and the formulation is tuned for infrared and laser welding.
Why the Calco grade works
- Heat-stabiliser package selected for retention of tensile strength after ageing at the OEM temperature
- Hydrolysis-resistant to survive fuel vapour, oil mist and EGR condensate
- Improved infrared and laser welding performance for two-shell designs
- High-flow variant for thin runner walls and long flow paths
- Controlled fibre length and orientation for weld-line strength at bosses
Which grade, when.
| Choose when | Calco grade | Construction | Family | What it gives you |
|---|---|---|---|---|
| Naturally aspirated, cost-driven, vibration welded | 710C3031 | PA6 GF30 | CiLON® | Toughness, weldability, lowest melt temperature |
| Turbocharged or hot-side EGR, continuous above 120 °C | 720C3001L | PA66 GF35 | CiLON® | Higher HDT and stiffness, heat stabilised |
| Thin runners, long flow, laser-welded shells | 720C3002HFHS | PA66 GF35 HF HS | CiLON® | High flow, laser weldability, aged strength |
How we validate it with you.
Burst on the welded assembly
Burst pressure on the welded manifold before and after heat ageing; weld factor on plaques welded on your process.
Thermal shock and vibration
Cycling between –40 °C and the engine-bay peak with pressure applied; vibration at the head flange with the gasket loaded.
Gate and weld-line placement
Mould-flow input so weld lines fall away from bolt bosses and the weld seam, and fibre orientation supports the flange.
More under the hood.
Air filter housings
Latch and hinge fracture once the polymer has embrittled with heat ageing.
OpenRadiator end tanks, cooling pipes and connectors
End-tank cracking at the crimp foot or hose spigot after coolant ageing.
OpenEngine covers and cylinder-head covers
Sink marks, fibre read-out and gloss variation on the visible engine cover.
OpenTry it on your own tool.