Home / Automotive / Under the hood / Cable ties
In production
Cable ties
The problem this part has to solve, what usually goes wrong, and the grade we recommend.
The problem your part has to solve.
A commodity part with the finest feature moulded in polyamide: the pawl in the head. Loop tensile strength is specified by class, the strap must wrap without cracking in a cold assembly hall, and ties routed through the engine bay must keep their strength after years at 105–125 °C. Tens of millions are moulded in 64- to 128-cavity hot-runner tools, so melt viscosity, fill consistency and cycle time decide the part cost as much as the polymer does.
Process: Injection moulding in high-cavity tools; moisture-conditioned before shipment.
What usually goes wrong
- Brittle straps from under-conditioned or over-dried material, or the wrong viscosity for the tool
- Pawl failure from short shots or flash in the head; flash on the strap from too-low viscosity
- Loss of loop tensile after heat ageing on engine-bay routings
- Strap cracking on wrapping at low ambient temperature
Our recommendation.
For general-purpose and interior routings we recommend CiLON® PA6, 710C0031A: PA6's toughness and elongation make the most forgiving strap, and its viscosity is set for high-cavity fill. For higher loop-tensile classes and higher temperature we recommend PA66, 720C0031A; for engine-bay routings specified for long-term heat ageing, PA66 HS, 720C0001HS; and for outdoor or cold-climate assembly, PA66 IM, 720C0003IM, whose impact modifier keeps the strap ductile at –40 °C. All four run on the same tools, so you can move between them as the routing changes.
Why the Calco grade works
- Toughness and elongation for strap flexibility and hinge performance
- Viscosity controlled lot to lot for consistent fill of the pawl in high-cavity tools
- Heat stabilisation that holds loop tensile after ageing at engine-bay temperature
- Impact modification for cold-climate assembly
- Excellent processability, short cycles and high fluidity
Which grade, when.
| Choose when | Calco grade | Construction | Family | What it gives you |
|---|---|---|---|---|
| General purpose and interior routings | 710C0031A | PA6 unfilled | CiLON® | Toughness, elongation, cost |
| Higher loop-tensile class and temperature | 720C0031A | PA66 unfilled | CiLON® | Strength and HDT |
| Engine-bay routings, long-term heat ageing | 720C0001HS | PA66 HS | CiLON® | Aged loop tensile |
| Outdoor and cold-climate assembly | 720C0003IM | PA66 IM | CiLON® | Ductility at –40 °C |
How we validate it with you.
Loop tensile by class
Loop tensile to IEC 62275 or your standard, dry-as-moulded, conditioned and after heat ageing.
Cold wrap
Strap wrapping and pawl engagement at –40 °C on ties conditioned to shipping moisture.
Cycle and fill on your tool
Fill balance, flash and cycle time on the customer's high-cavity tool; viscosity window agreed and held.
More under the hood.
Air intake manifolds
Flange cracking after thermal cycling where weld lines and fibre orientation meet the bolt bosses.
OpenAir filter housings
Latch and hinge fracture once the polymer has embrittled with heat ageing.
OpenRadiator end tanks, cooling pipes and connectors
End-tank cracking at the crimp foot or hose spigot after coolant ageing.
OpenTry it on your own tool.
A free 25 kg trial lot compounded on production lines, and a Calco engineer at your press.
